Researchers in China tested 16 optical channels on one chip, each at 224 gigabits per second. The experiment puts a thin ceramic film in contention for the high-speed links that connect computing equipment.

Fibre-optic distribution equipment for home connections.
Fibre-optic equipment used to connect homes. Illustrative photograph by Ronald Crow / Unsplash.

Sixteen green traces on an oscilloscope tell the story of a new optical transmitter. Each trace comes from a different wavelength of light and records how clearly a receiver could distinguish a rapidly changing signal. In measurements published on Friday, all 16 channels on the chip produced readable patterns at 224 billion bits per second apiece.

The device was built by researchers in Beijing and Hangzhou. They patterned it on an eight-inch silicon wafer coated with a thin layer of lead zirconate titanate, a ceramic usually shortened to PZT. On that material they made both the paths that guide light and the components that imprint an electrical signal onto it.

The team describes the transmitter as a candidate for links in the 3.2-terabit-per-second class. That figure refers to the combined capacity of multiple channels. The laboratory tests measured signal quality. The useful data rate between two computers would also depend on the receiver, error correction and network equipment.

Different wavelengths can share a strand of glass and still be separated at the receiving end. Engineers call this wavelength-division multiplexing. The wavelengths used for optical communications lie in the infrared, outside human vision. Calling each one a colour is a convenient way of describing how a receiver can tell them apart.

A data centre switch has limited space for fibre connections on its front panel. Putting several streams of information on each fibre can increase the traffic that fits through those connections. It also puts more work on the chip that keeps the streams separate.

How to put two bits on a flash of light

An optical transmitter needs a way of converting an electrical message into changes in light. The ceramic helps because an electric field changes the speed at which light travels through it. The change is small, but with the right arrangement of paths it can make a large difference to the brightness emerging at the far end.

The researchers divided light between two short arms and then brought the beams back together. Changing the voltage makes one set of light waves arrive at a slightly different point in its cycle relative to the other. Where the waves reinforce one another, the output brightens. Where they cancel, it dims.

There is more than one way to use that dimmer. Switching between two brightness levels allows each signal interval to carry a single bit. The team also used four levels, enough to represent the four possible pairs of binary digits. At 112 billion intervals per second, that produces the reported 224 gigabits on an individual channel.

The price of those extra bits is a finer distinction for the receiver to make. A pulse that is clearly brighter than the darkest level might still be difficult to distinguish from the next level up. Noise, distortion or an error in when the receiver samples the pulse can blur the boundary between them.

An oscilloscope makes that boundary visible by drawing many short stretches of the received signal on top of one another. Four well-separated levels leave three open spaces in the trace. Engineers call these openings eyes. Their size gives a sense of how much leeway the receiver has when picking the level and the instant to read it.

The researchers examined those patterns across all 16 wavelengths. Each wavelength has to pass through the same separator. If a component sends too much light into a neighbouring channel, the unwanted signal competes with the one the receiver is trying to read.

Making light turn a corner

The ceramic itself has a memory that helps the modulator. Tiny regions within the film can point their electrical polarisation in different directions. The researchers applied a field to line them up. Some alignment remains after the field is removed, leaving the material more responsive when the high-speed electrical signal arrives.

Other researchers have used this property before. In 2018 a group at Ghent University and its partners reported 40-gigabit-per-second signals from devices that combined PZT with silicon nitride. The Belgian result showed how the ceramic could change light on a chip. The new work puts the modulating elements beside the components that direct a much larger set of signals.

One such component separates incoming light by wavelength. It sends the light through an array of paths of slightly different lengths. When the light emerges, waves of a particular wavelength reinforce one another at a particular outlet. That arrangement delivers each colour to its own modulator, even though the colours arrived at the device together.

This makes the geometry of the wafer unusually important. If light propagates differently when a path turns through an angle, the intended timing can slip. Designers then have less freedom to place components wherever they fit. The researchers tested otherwise identical structures at several orientations to see how much their optical behaviour changed.

The small dependence they found on orientation gives designers latitude to route paths around one another. That is a practical advantage when placing a row of modulators alongside a wavelength separator. It is also one reason a circuit designer might choose a material for qualities that never appear in a headline speed figure.

There is a related manufacturing issue. A laboratory can spend considerable effort finding one well-behaved component on a sample. Fabricating useful chips across an eight-inch disc requires the coating and the etched features to behave consistently from place to place. The team measured structures from different parts of its wafer to check that consistency.

From a laboratory trace to a network link

Another test addressed the point where the chip meets an optical fibre. Light confined to a tiny path on the wafer must transfer into a fibre of a different size and shape. The researchers used computed patterns of grooves to direct light across the interface and measured how much optical power survived the trip.

Every loss at a connection comes out of the same power budget. The laser must send enough light for the receiver to distinguish four levels after the signal passes through the chip, the connectors and the fibre. A design that performs well on one short path may have less margin when other components are added.

Speed alone also says little about the electricity a finished link will use. The electrical driver, laser, receiver and signal-processing circuits all consume power. To compare two products, a network operator would want the consumption of the whole link at the same distance and error rate. A measurement of the modulating element answers a narrower engineering question.

The team did test how its modulators behaved over time and across changing temperatures. The ceramic needs to retain its electrical alignment. A packaged device would also have to preserve the alignment between fibre and chip as it heats up and cools down in service.

Adding more wavelengths is one way to raise capacity further. Packing them closer together would make more efficient use of the available spectrum, but it would also leave less room for errors in separating them. Small deviations in fabrication become more consequential when the intended signal and its neighbour sit closer together.

For now, the clearest result is visible in that set of traces. The researchers made 16 devices on one circuit, sent a different infrared wavelength to each and showed the signal that emerged from every channel. The next revealing measurement would follow the same data farther, through a packaged link to a receiver at the other end.